Sintering Carbon
Sintering process Carbon bush , Shaft dimension from 24mm to 55mm Press to Size then Vacuum furnace sinterized by 1600 ℃ degree High bending strength and denstiy then normal impregnated carbon ...
We are here to solve your problems professionally
Contact Now
- Tel:0086-21-58355541
- Fax:0086-21-58353141
- Email: trisun24@trisunltd.com(sales)
Sintering process Carbon bush , Shaft dimension from 24mm to 55mm
Press to Size then Vacuum furnace sinterized by 1600 ℃ degree
High bending strength and denstiy then normal impregnated carbon

Press to Size then Vacuum furnace sinterized by 1600 ℃ degree
High bending strength and denstiy then normal impregnated carbon

You can fill out the form below to send your contact information and product demand submitted to us. We will solve as soon as possible! Thank you! To be able to contact you promptly and make sure you complete the full contact and demand information